The Effects of Exposure to Sea Water Steam on Thermal Conductivity of Varnished Fir Wood
Küçük Resim Yok
Tarih
2012
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Kastamonu Univ, Orman Fak
Erişim Hakkı
info:eu-repo/semantics/closedAccess
Özet
In this study, the thermal conductivity of varnished fir wood exposed to sea water steam was investigated. For this purpose, test samples were coated by using varnishing goldspar (polyurethane varnish), original (synthetic varnish), perfection (polyurethane varnish), and schooner varnishes (synthetic varnish). After applying furnished process, samples were exposed to sea water steam during 6, 24, 60, and 96 hours. It was found that the vapour application has decreased the chemical and physical structure of test material. The thermal conductivity test was performed based on the ASTM C 1113-99 hot-wire method.
Açıklama
Anahtar Kelimeler
Wood, Varnish, Thermal Conductivity
Kaynak
Kastamonu University Journal of Forestry Faculty
WoS Q Değeri
N/A
Scopus Q Değeri
Cilt
12
Sayı
3