Atık plastiklerin demir cevherinin indirgenmesinde kullanılabilirliğinin araştırılması

dc.contributor.advisorCandan, Ercan
dc.contributor.authorErtan, Serap
dc.date.accessioned2024-09-29T18:37:35Z
dc.date.available2024-09-29T18:37:35Z
dc.date.issued2009
dc.departmentLisansüstü Eğitim Enstitüsü, Metal Eğitimi Ana Bilim Dalıen_US
dc.descriptionFen Bilimleri Enstitüsü, Metal Eğitimi Ana Bilim Dalıen_US
dc.description.abstractBu çalışmada, polietilen (PE), polipropilen (PP) ve akrilonitrilbütadienstiren (ABS) atık plastiklerinin geri dönüşümü kapsamında demir cevherinin indirgenmesi çalışılmıştır. Demir cevheri olarak % 51,68 metalik demir oranına sahip manyetit cevheri kullanılmıştır. Çalışmalarda 1/2-1,0-1,5-2,0 saat sinterleme süresi, 1200, 1250, 1300 0C sinterleme sıcaklığı, % 5, % 10, % 15, % 20, % 25 oranlarında cevhere atık plastik parametreleri incelenmiştir. Ayrıca, cevher tozu tane boyutuna bağlı indirgenme özellikleri de bu çalışmada incelenmiştir.Deneysel sonuçlar; atık plastiklerin demir cevheri indirgenmesinde kullanılabileceğini göstermiştir. İndirgenme için optimum sinterleme sıcaklığı 1250 0C, sinterleme süresinin ise 1,5 saat olduğu gözlenmiştir. İndirgenme işleminde atık plastiğin çeşidine göre indirgenme miktarı değişmiştir. PE ve PP için optimum karışım miktarı % 10 iken ABS için bu oran % 25 olduğu sonucuna varılmıştır.Mikroyapı çalışmaları indirgenme sonrasında elde edilen yapının yüksek karbonlu çeliklere benzediğini göstermiştir.en_US
dc.description.abstractIn this study, reduction of iron ore by using waste plastics, such polyethylene (PE), polypropylene (PP) and acrylonitrilebutadienestyrene (ABS), has been investigated. Magnetite type iron ore with 51,68 % metallic content has been used. Sintering duration of 1/2-1,0-1,5-2,0 h., sintering temperature of 1200, 1250, 1300 0C and the waste plastics at the ratios of 5-10-15-20 and 25 % were used for the reduction processing. Additionally, the reduction as a function iron ore particle size has also been investigated.Experimental studies showed that the waste plastics used in this study could be successfully used for the reduction of iron ore. It was observed that ideal sintering temperature was 1250 0C while the optimum sintering duration was 1,5 h. The ratio of waste plastics in the mixture was varied according to its plastic type. The ideal mixture was 10 % for the PE and PE where as it was 25 % for the ABS.Microstructural examinations showed that the microstructure was similar to that of high carbon steels.en_US
dc.identifier.endpage106en_US
dc.identifier.startpage1en_US
dc.identifier.urihttps://tez.yok.gov.tr/UlusalTezMerkezi/TezGoster?key=UPP_Zu9isEmWGFXFCBYasVrp0H--NZHDJZbTZw8uLDr0jFjGn483hu6SpOSzUjcW
dc.identifier.urihttps://hdl.handle.net/20.500.14619/14327
dc.identifier.yoktezid237715en_US
dc.language.isotren_US
dc.publisherKarabük Üniversitesien_US
dc.relation.publicationcategoryTezen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectMetalurji Mühendisliğien_US
dc.subjectMetallurgical Engineeringen_US
dc.titleAtık plastiklerin demir cevherinin indirgenmesinde kullanılabilirliğinin araştırılmasıen_US
dc.title.alternativeAn investigation on usage of waste plastics on reduction of iron oreen_US
dc.typeMaster Thesisen_US