Catalytic pyrolysis of waste melamine coated chipboard

Küçük Resim Yok

Tarih

2013

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Wiley-Blackwell

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Özet

Catalytic pyrolysis of waste melamine coated chipboard was performed in a fixed-bed reactor at 400 degrees C, 500 degrees C, 600 degrees C, and 700 degrees C and a residence time of 1 h. The effects of temperature and catalysts on both product distribution and bio-oil composition were discussed. Lewis acids (AlCl3, TiCl4, and FeCl3), bases (NaOH and KOH), and basic salts (Na2CO3 and K2CO3) were used as catalysts in the pyrolysis process. The product distributions were changed depending on both the type of catalyst and temperature. Bio-oil obtained from the pyrolysis of melamine coated chipboard contained a large variety of oxygenated hydrocarbons. Phenols were found to be the major compounds identified in bio-oils for all tested runs. The bio-oils produced by Lewis acids contained aldehydes. However, the bio-oils obtained from the thermal run, the run with bases, and the run with basic salts did not contain these compounds. (c) 2011 American Institute of Chemical Engineers Environ Prog, 32: 156161, 2013.

Açıklama

Anahtar Kelimeler

melamine coated chipboard, pyrolysis, bio-fuel, biomass

Kaynak

Environmental Progress & Sustainable Energy

WoS Q Değeri

Q3

Scopus Q Değeri

Q2

Cilt

32

Sayı

1

Künye