The Wear Properties of In-Situ 7075 Al-Ti Composites Produced by Powder Metallurgy Route
dc.authorid | YILDIRIM, MUSA/0000-0002-2464-1182 | |
dc.contributor.author | Ay, H. | |
dc.contributor.author | Ozyurek, D. | |
dc.contributor.author | Yildirim, M. | |
dc.contributor.author | Bostan, B. | |
dc.date.accessioned | 2024-09-29T16:01:10Z | |
dc.date.available | 2024-09-29T16:01:10Z | |
dc.date.issued | 2016 | |
dc.department | Karabük Üniversitesi | en_US |
dc.description | 5th International Advances in Applied Physics and Materials Science Congress and Exhibition (APMAS) -- APR 16-19, 2015 -- Oludeniz, TURKEY | en_US |
dc.description.abstract | In this study, the wear properties of in-situ 7075 Al-Ti composites produced by powder metallurgy route were investigated. Different amount of Ti (2, 4, 6 %) added to gas atomized 7075 Al alloy powders and they were mixed in turbula with 47rpm for 45 minutes. Then the mixed powders were pre-shaped by press under 600 MPa pressure. The samples were cooled in the furnace after sintered at 580 degrees C for 4 hours in the atmosphere controlled furnace. Standard metallographic process such as grinding, polishing and etching were applied to sintered samples. The hardness values were measured. Scanning Electron Microscope (SEM), X-Ray Diffraction (XRD) examines were carried out. The wear tests were performed in a pin-on disc type wear apparatus with 1 ms(-1) sliding speed at six different sliding distance (500-3000 m) under 30 N loads. As a result of studies, hardness values were increased with increasing Ti content, in addition the weight losses were decreased with increasing Ti amount. | en_US |
dc.identifier.doi | 10.1063/1.4945956 | |
dc.identifier.isbn | 978-0-7354-1374-0 | |
dc.identifier.issn | 0094-243X | |
dc.identifier.scopus | 2-s2.0-84984548687 | en_US |
dc.identifier.scopusquality | N/A | en_US |
dc.identifier.uri | https://doi.org/10.1063/1.4945956 | |
dc.identifier.uri | https://hdl.handle.net/20.500.14619/5559 | |
dc.identifier.volume | 1727 | en_US |
dc.identifier.wos | WOS:000375930200001 | en_US |
dc.identifier.wosquality | N/A | en_US |
dc.indekslendigikaynak | Web of Science | en_US |
dc.indekslendigikaynak | Scopus | en_US |
dc.language.iso | en | en_US |
dc.publisher | Amer Inst Physics | en_US |
dc.relation.ispartof | Proceedings of the 5th International Congress in Advances in Applied Physics and Materials Science Congress & Exhibition (Apmas '15) | en_US |
dc.relation.publicationcategory | Konferans Öğesi - Uluslararası - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Ti | en_US |
dc.subject | Wear properties | en_US |
dc.subject | 7075 Al alloy | en_US |
dc.subject | In-situ composites | en_US |
dc.subject | Powder metallurgy | en_US |
dc.title | The Wear Properties of In-Situ 7075 Al-Ti Composites Produced by Powder Metallurgy Route | en_US |