Wear behavior of severe shot peened and thermally oxidized commercially pure titanium

Küçük Resim Yok

Tarih

2019

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Springer Verlag

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Özet

In this study, severe shot peening (SSP) has been performed to commercially pure titanium (Grade 2) specimens in order to expose severe plastic deformations to the material surface. S230 shot media with higher air pressure conditions have been selected for SSP. A nanocrystalline layer has been created by means of severe plastic deformation. The nanograined structure has been investigated via XRD, FESEM, and microhardness methods. SSP specimens have been subjected to thermal oxidation treatment in air at 500 and 700 °C for 2 and 16 h. Severe shot peened commercially pure titanium has a thicker oxide layer when compared to as received ones. The results show that both SSP and thermal oxidation improve the wear characteristics. © 2019, Springer International Publishing AG, part of Springer Nature.

Açıklama

Anahtar Kelimeler

Nanograined layer, Severe shot peening, Thermal oxidation, Wear

Kaynak

Advanced Structured Materials

WoS Q Değeri

Scopus Q Değeri

N/A

Cilt

92

Sayı

Künye